Skip to main content
Fig. 5 | Stem Cell Research & Therapy

Fig. 5

From: Polymer-mineral scaffold augments in vivo equine multipotent stromal cell osteogenesis

Fig. 5

Three-dimensional explant reconstructions demonstrating models generated with high (left) and low (right) thresholds to distinguish between high contrast scaffold structure (left) versus low contrast newly deposited tissue (right). A single threshold was used for GA constructs due to the limited presence of high contrast material in the specimens. ASC adipose-derived multipotent stromal cell, BMSC bone marrow-derived multipotent stromal cell, GA polyethylene glycol (PEG)/poly-l-lactic acid (PLLA), GT PEG/PLLA/tricalcium phosphate (TCP)/hydroxyapatite (HA), HT TCP/HA

Back to article page