Fig. 3From: Bioengineered skin constructs based on mesenchymal stromal cells and acellular dermal matrix exposed to inflammatory microenvironment releasing growth factors involved in skin repairhADM biocompatibility and construct formation. SEM shown the hWJ-MSCs attachment on hADM, scale bar = 30 μm (A), and Hematoxylin and Eosin staining (B) shown the infiltration of hWJ-MSCs inside hADM scaffold, scale bar = 100 μm, as indicated by arrows, respectively. In recellularized hADM, the viability of hWJ-MSCs (green) was more than 98% after 24 h, scale bar = 100 μm (C). Resazurin-based assay to monitor the proliferation of hWJ-MSCs on hADM (two donors: hADM1 and hADM2) during the culture process (D), values were normalized using a control group (cells grown on TCP). n = 3, p < 0.05. TCP tissue culture plateBack to article page